http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1507828-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_adb0e564374fedf34b36103d36e6455a |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-18 |
filingDate | 2003-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1917488cfe61c42cd8ac5adef9bd0b4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5dec37868fc39c541fd620609af165eb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_082ec901b088f60bb672ee53d5e0ea64 |
publicationDate | 2005-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-1507828-A1 |
titleOfInvention | Process for making a thermoplastic composition comprising dynamic cross-linking |
abstract | The invention relates to a process for making a thermoplastic composition comprising dynamic cross-linking of a composition comprising a thermoplastic matrix polymer A having functional groups reactive with epoxide groups and 25-80 mass% based on polymer A of a polymer B having epoxide groups and secondary hydroxyl groups, and optionally other components. This process omits separate addition of a cross-linking agent, because the polymer B is self-crosslinking above a certain temperature. A further advantage is that the risk of undesired side-reactions, e.g. leading to degradation of polymers in the blend is reduced. Another advantage is that cross-link density of polymer B can be varied up to relatively high cross-link densities, by varying the total amount of functional groups or the ration of epoxide to secondary hydroxyl groups. With this process products with improved properties are obtained. The invention further concerns the product obtainable by said process, and use thereof as the thermoplastic elastomer or impact-modifier. |
priorityDate | 2002-05-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 57.