http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1483324-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_da32d5d37133cae4ea6513b5876be7aa |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2308-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-142 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-654 |
filingDate | 2003-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f6d59bea3b32fbb9ee8b11526c94d49 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14e5fa1c82e264f9b9e9723669382fc9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d9f6d44623d34301bbde990f9fc09b23 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c13b68d60912e1e476e972ac2b22c26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_529eb5e62a0e77c6277156c731790206 |
publicationDate | 2004-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-1483324-A1 |
titleOfInvention | Polyolefin compositions having high tenacity |
abstract | A polyolefin composition suitable for preparing single ply roofing membranes, comprising: (A) from about 15 to 40% by weight of a crystalline copolymer of propylene with at least one alpha-olefin of formula H2C=CHR1, where R1 is H or a C2-8 linear or branched alkyl, containing at least about 90% by weight of propylene, having solubility in xylene at room temperature lower than about 15% by weight; (B) from about 60 to about 85% by weight of an elastomeric fraction comprising: (1) a copolymer of propylene with ethylene containing about 20 to about 35% by weight ethylene, and having solubility in xylene at room temperature greater than about 70% by weight, the intrinsic viscosity of the xylene soluble fraction being higher than about 3.0dl/g; and (2) a copolymer of ethylene with at least one alpha-olefin of formula H2C=CHR2, where R2 is a C2-8 linear or branched alkyl, containing about 15% to 40% by weight alpha-olefin, and having solubility in xylene at room temperature greater than about 25% by weight, the intrinsic viscosity of the xylene soluble fraction ranging from about 0.5 to about 5.0dl/g; the (1) (2) weight ratio ranging from about 1:5 to about 5:1. The polyolefin composition of the invention, preferably prepared by sequential polymerization in at least three stages, has tensile strength at break ≥ 25 Mpa, elongation at break ≥ 700 Mpa and toughness ≥ 150 Mpa. |
priorityDate | 2002-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |