Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_294b2f418bb67c546f940251156d0c86 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J175-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B24B13-0055 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J151-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F265-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J4-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00942 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B24B13-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J151-003 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02C7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29D11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J151-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J151-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J175-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B24B13-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J4-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-04 |
filingDate |
2002-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fe79a89c0ca908a25d05cc8fa0abb401 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b55da7c5553f0195bcfe6cddc5a4217 |
publicationDate |
2004-06-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-1423234-A2 |
titleOfInvention |
Method, apparatus and adhesive composition for ophthalmic lens blocking |
abstract |
A method is provided for blocking a lens according to which a lens block (210) is obtained which transmits UV and visible light. An adhesive curable by light within the UV and visible spectrum is applied between the lens blank (60) and a lens mounting face of the lens block (210). The lens blank (60) is placed adjacent the lens block (210) with the adhesive extending therebetween. UV light is applied to cure the adhesive. The adhesive is selected to have a suitable low dimensional change on setting so as not to impart any undue stresses on the lens blank which being capable of total adhesive failure without lens damage or leaving a residue upon application of a suitable stripping force. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023073249-A1 |
priorityDate |
2001-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |