http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1398149-B1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8aa5b8d694dc73c3e0d5a69c0c314218
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D75-305
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-32
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-185
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D75-30
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-34
filingDate 2002-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 2007-05-02-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_681dfdf743cc105c02447b053a40653f
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9c6c241d42b043da18ebf689cace2bc3
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2b45b68cd9ff33316d29aa150c4a7a49
publicationDate 2007-05-02-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber EP-1398149-B1
titleOfInvention Printable thermoplastic multilayer laminate for vacuum skin packaging applications
abstract A printable thermoplastic multilayer laminate is a coextruded and multilayered laminate, and comprises a polyolefin sealing layer (1), a gas-barrier layer (4) and/or a resin material layer. The laminate has modulus of 4000 kg/cm2> or more at room temperature of 23[deg]C. The resin material layer has glass transition temperature of 70-150[deg]C, more preferably 70-100[deg]C, and tensile modulus of 1900 MPa or more. A printable thermoplastic multilayer laminate is a coextruded and multilayered laminate, and comprises a polyolefin sealing layer, a gas-barrier layer and/or a resin material layer. The multilayer laminate has modulus of 4000 kg/cm2> or more at room temperature of 23[deg]C. The resin material layer has glass transition temperature of 70-150[deg]C, preferably 70-125[deg]C, and more preferably 70-100[deg]C, and tensile modulus of 1900 MPa or more evaluated according to ASTM D882 on a sheet (250 mu m). Independent claims are included for the following: (1) vacuum skin packaging process which involves using the multilayer laminate as top skin web; (2) vacuum skin package comprising a support, a product positioned on the support, and coextruded multilayer laminate covering the product, conforming to its shape and sealing to the support around periphery of the product.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10934070-B2
priorityDate 2002-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID250594
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID135677588
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID12510961
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID54137699
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID128851202
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID129155308
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID128774372
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID128900508

Total number of triples: 30.