http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1357091-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_44ff3005508304394801e265e503b811 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-21 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-21 |
filingDate | 2001-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cf7f4e9b381716e7056a4e0b58f46ea3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_068609a1dd082b4f2f49e637ceda4c73 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e1112ad0a6539aed4580790347ec4f1f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2ad7148cabef5be195731ee41f91a4fd |
publicationDate | 2003-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-1357091-A1 |
titleOfInvention | Optical glass and optical product using the same |
abstract | Provided is an optical glass having a high refractive index and high dispersion characteristics applicable to mass production of precision press molded products, mainly having optical constants of a refractive index nd in the range of 1.7 to 2.0 and an Abbe number nu d in the range of 20 to 32, and an optical part and a precision press molding material. An optical glass comprising as glass components, as molar percents, 12-34 percent of P2O5; 0.2-15 percent of B2O3 (where the total quantity of P2O5 and B2O3 is 15-35 percent); 0-45 percent of WO3; 0-25 percent of Nb2O5; 0 to 10 percent of TiO2 (where the total quantity of WO3, Nb2O5, and TiO2 is 20-45 percent); 0-25 percent of BaO; 0-20 percent of ZnO (where the total quantity of BaO and ZnO is less than 30 percent); 2-30 percent of Li2O; 2-30 percent of Na2O; 0-15 percent of K2O (where the total quantity of Li2O, Na2O, and K2O is 10-45 percent); 0-10 percent of CaO; 0-10 percent of SrO; 0-5 percent of Al2O3; 0-5 percent of Y2O3; 0-1 percent of Sb2O3; and 0-1 percent of As2O3; where the total quantity of all of the above-listed components is equal to or more than 94 percent. An optical part or precision press molding material comprised of this optical glass. <IMAGE> |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102849945-A |
priorityDate | 2000-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 47.