Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ec0302f0e906bc6b19a4194d12264f89 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J11-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J11-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J9-242 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J11-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J11-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J9-02 |
filingDate |
2001-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f4f21fb36991a24f45d98f4bfc36016f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d70bdf365fe744540a1102e9d97e212e |
publicationDate |
2003-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-1354331-A1 |
titleOfInvention |
Process for manufacturing barriers for a plasma display panel |
abstract |
Process comprising the following steps: a) deposition of a green layer based on 0.1% to 8% of an organic binder, on a mineral filler and on 0.1% to 13% of a mineral binder; b) formation of the barriers by spraying an abrasive material onto a mask applied against this layer, and then removal of the mask; c) deposition of a phosphor-based green layer; d) baking of the two layers, preferably simultaneously. By virtue of the limited amount of organic binder, the abrasion rate is high; if this content is at least 2%, deterioration of the green barriers is avoided. |