http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1290075-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0efa077d881a96aeb1e29b21ef1bbb58 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L55-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-005 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-02 |
filingDate | 2001-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ab2a1756df1952d7f6130fed5166a864 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fcc6e3cc6493e619ade1e9dd8857272a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_195737f968fc7c12c066508e8dc7fb5b |
publicationDate | 2003-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-1290075-A1 |
titleOfInvention | Stabilized thermoplastic moulding materials |
abstract | Thermoplastic moulding materials containing the following ingredients with regard to components A-F: A) 5-70 wt. % of at least one graft copolymer A) consisting of a rubber elastic base with a glass transition temperature below 0 DEG and a grafted overlay made of a styrene compound and acrylonitrile or methacrylonitrile or mixtures thereof in addition to, optionally, other monoethylenically unsaturated monomers, B) 29 - 90 wt. % of a hard copolymer made of at least one styrene compound, acrylonitrile or methacrylonitrile or mixtures thereof and, optionally, other monoethylenically unsaturated monomers, C) 0 - 5 wt. % of at least one three-block copolymer X-Y-X with a middle block Y made of propylenoxide units and terminal blocks X made of ethylenoxide units, D) 0.01 - 5 wt. % of at least one butylated reaction product of cresol with dicyclopentadiene, E) 0.01 -5 wt. % of at least one thiocarboxylic acid ester, F) 0.01 -5 wt. % of at least one alkaline metal salt or alkaline earth metal salt of a C6-C20carboxylic acid, G) 0 -30 wt. %, in relation to constituents A) - G), of other usual additives. The moulding materials exhibit a db*-value, after exposure to the atmosphere, of less than +5,0 after 100 hours of exposure to light and the atmosphere according to ISO 4892/2, method A, black panel temperature 65 DEG C, colour measurement according to CIE-Lab in accordance with DIN 6174 and DIN 5033. |
priorityDate | 2000-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |