http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1231951-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_21e6d1c28c65452db152a4542c696506 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L2400-18 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-56 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61F2-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L27-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L27-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F3-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L27-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B38-00 |
filingDate | 2000-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2005-11-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_59660453dea06d96c10051b34f179bdc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d97819f2664c08d109af75829f156d8c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_faba5359292130573fac0b40a43fe37d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f709ce038b447d42352629d2d32f8a5c |
publicationDate | 2005-11-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-1231951-B1 |
titleOfInvention | Process for producing rigid reticulated articles |
abstract | A process for producing a rigid reticulated article, includes: (a) providing a first dispersion of a ceramic or metal powder, a binder, and a solvent; (b) providing a reticulated substrate which has open, interconnected porosity; (c) contacting the reticulated substrate with the first dispersion to coat the substrate with the dispersion to form a first coating; (d) drying the coated reticulated substrate; (e) contacting the reticulated substrate with one or more additional dispersions to form one or more additional coatings wherein the composition of the one or more additional coatings are the same or different from each other and the first coating; (f) drying the additional coating between the steps of contacting; (g) heating the coated reticulated substrate at a time and temperature sufficient to pyrolyze any organic components; and (h) sintering to form a ceramic or metal or composite reticulated article. In another aspect, the binder becomes solvent-insoluble and flexible upon drying. According to this aspect, one or more additional coatings may optionally be used. |