Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2200-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-498 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-49845 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-061 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-04 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-49863 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 |
filingDate |
2001-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ec8db15d25b66ce5c13d909bcbbbc3c7 |
publicationDate |
2002-06-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-1215530-A2 |
titleOfInvention |
Silver salt photothermographic material |
abstract |
A silver salt photothermographic material isndisclosed, comprising on a support a light-sensitive layerncomprising an organic silver salt, light-sensitive silvernhalide grains, a reducing agent and a binder, wherein afternthe photothermographic material having been developed at antemperature of not less than 100° C is subjected to exposurento light of an illumination intensity of 300 lux at 45° Cnfor 24 hrs., the rate of variation in fog density betweennbefore and after exposure is not more than 30%, based on thenfog density of the photothermographic material beforenexposure. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1241520-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1241520-A2 |
priorityDate |
2000-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |