abstract |
A poly-1-butene resin composition comprising:n 90 to 99.95% by weight of a poly-1-butene resin (A) obtainable byn(co)polymerizing 80 to 100% by mol of 1-butene and 0 to 20% by mol of an α-olefinnof 2 to 10 carbon atoms other than 1-butene and having a melt flow rate (MFR;nASTM D 1238, 190 °C, load of 2.16 kg) of 0.01 to 50 g/10 min, and 0.05 to 10% by weight of a polypropylene resin (B) having a melt flow raten(MFR; ASTM D 1238, 230 °C, load of 2.16 kg) of 0.01 to 50 g/min. |