http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1211232-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d811ffcbe0dc861b62b4db33c0528244 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C06B33-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C06B21-0058 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C06B21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C06B33-08 |
filingDate | 2001-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_60e49b5112ab84a44d72480cf4c676dc |
publicationDate | 2002-06-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-1211232-A2 |
titleOfInvention | Process for producing mouldable, plastic-bound explosives |
abstract | The invention relates to a method for producing castable plastic-boundnExplosive charges, where a crystalline explosive into a polymer matrix from anBinder, a plasticizer and other auxiliaries is embedded.n n n In order to achieve that the explosive charge despite a high (e.g. 90%) solid contentnremains pourable and therefore has a sufficiently low viscosity without firstnsieving out the grain fraction of the explosive crystals is required by the inventionnbefore, the explosive charge 0.1 to 10 wt .-% fine-grained vanadium, niobium, tantalum,nChromium, molybdenum or tungsten powder or a mixture of two or morento add such powders, the powder grains of the respective metal powdernshould have a substantially spherical shape. Surprisingly, it has been shownnthat such metal powders as liquid lubricants between the coarser onesnExplosive particles act and reduce the viscosity of the correspondingnCause explosive charge. |
priorityDate | 2000-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |