abstract |
The polyamide resin shaped article of the present invention is produced by preliminarily melt-kneading a m-xylylene-containing polyamide resin and a layered silicate subjected to a swelling treatment to prepare a resin composition containing the layered silicate in high concentration, melt-kneading the resin composition with another portion of m-xylylene-containing polyamide resin, and then formed into the shaped article. Since the amount of the m-xylylene-containing polyamide resin exposed to the heat history twice in the melt-kneading steps is minimized, the gel formation due to the thermal degradation can be reduced and the lowering of the relative viscosity due to the decrease of the molecular weight caused by the thermal degradation of the m-xylylene-containing polyamide resin is prevented. |