Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_38a0ecf90a4ec02af686213ff43d2a9e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F2998-10 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F42B7-046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F42B12-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C1-045 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F42B7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F42B12-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C1-04 |
filingDate |
2001-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_40223b39b39daae701901b49665f9911 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2945082e17ddb428a7adc5272a055cf6 |
publicationDate |
2001-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-1154026-A1 |
titleOfInvention |
Process for preparing composite tin-tungsten shot of small dimension |
abstract |
The subject of the invention is a methodnparticularly simple and inexpensive to manufacturenof tin-tungsten composite elements having anthickness between 1 mm and 6 mm, such asnspherical shot for hunting cartridges or pelletsnpeach, from a mixture of tin powders andntungsten.n n n The powder mixture is directly extruded, atnsolid state, in a wire whose thickness is includednbetween 1 mm and 6 mm with a spinning speed ≤ 80 mm / s.n n n The wire is then cut into sections which arenthen stamped into the desired shape, in particular bynspheres.n n n The invention also relates to the processnaforementioned obtaining the wire. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7837809-B2 |
priorityDate |
2000-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |