Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_076e464be266dd9fabcd6d7fd96cc99e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2323-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2325-022 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2325-026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2323-08 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D69-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D67-0018 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D67-0027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D67-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D69-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D71-26 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D69-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D69-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D69-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D71-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-22 |
filingDate |
2000-01-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3d9e3913d69420382fbb8adde29e8365 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6c92db9aa27e2466518b634d9fea7e74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9f58ea9863a4c7b3a3a41d03b7ac40f5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e31a1b5d88237dff0f78dca86e8ddb95 |
publicationDate |
2001-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-1140331-A1 |
titleOfInvention |
Method for producing an integrally asymmetrical polyolefin membrane |
abstract |
The invention relates to a method for producing an integrally asymmetrical hydrophobic polyolefinic membrane with a sponge-like, open-pored microporous support structure and an separating layer with a structure which is denser than the support structure, by means of a thermally induced liquid-liquid phase separation process. A solution of at least one polyolefin in a solvent system consisting of a compound A and a compound B, is extruded to obtain a shaped body. Compound A is a weak solvent and compound B is a non-solvent for the polymer. After leaving the moulding tool, the shaped body is cooled using a solid or liquid cooling medium which will not dissolve the polymer at temperatures up to the temperature of the tool and which will not chemically react with the polymer, until phase separation occurs and the polymer-rich phase hardens. |