Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a8e2962a998e1c197903e9b3cd0d4b67 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C9-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C9-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C9-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C9-04 |
filingDate |
2000-06-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_17dc3ea5e010fb1b2ef5b0c2cdee7ea7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b5f988f787b564d2b66b5417ce2bba7c |
publicationDate |
2000-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-1061147-A1 |
titleOfInvention |
Use of a copper-tin-iron alloy |
abstract |
The invention relates to the use of a copper-tin-iron alloy which consists of 4nup to 12% tin; 0.1 to 4% iron; Balance copper and usual impuritiesnexists for the production of joined components, such as jewelry in particular,nClothing accessories or glasses etc. |
priorityDate |
1999-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |