abstract |
A process for melt-spinning solution-polymerized polyurethanes, based on polyether glycols and MDI at an addition ratio of 1.8 to 6.0, glycol chain extenders and a chain terminator to produce number average molecular weights of the polyurethanes of 40,000-150,000, and 5-2500 decitex spandex made thereby, are provided. |