Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be2258efa1dd0212d91e87b0487f4ede |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-045 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K8-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-08 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K8-46 |
filingDate |
1999-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bf4cca304de26eaf7c3193def9a8211c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bddf8be3dc6a1002448d2dfc9fbf84f0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_536c58e4e65f8b45ca82ca9c0bed67a7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_549e3531115c37b28d01c51da09fe8cf |
publicationDate |
2000-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0969182-A2 |
titleOfInvention |
Well sealing composition and method |
abstract |
A well sealing composition comprises slag cement and the followingncomponents present in an amount by weight of slag cement in the composition:n8-20% slag cement activator; 30-60% water; 3-50% a hardenable epoxidencontaining material; and 2-40% an epoxide containing material hardening agent. |