http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0954551-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0efa077d881a96aeb1e29b21ef1bbb58 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F279-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F265-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-022 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-04 |
filingDate | 1998-01-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_08439f4f9ae20797c1d29db47d04acf1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a55574495ede1ea2354c4e6738c4985 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c46e24026c658c4b92402482689760f0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bc9d5e7c9f00c7d1fe9afec5b7f8c060 |
publicationDate | 1999-11-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0954551-A1 |
titleOfInvention | High-tenacity thermoplastic moulding materials |
abstract | The invention relates to thermoplastic moulding materials containing A) 30-98 wt.% of a thermoplastic polymer comprising, in relation to A), a1) 50-100 wt.% of a styrene compound of general formula (I), in which R?1 and R2¿ stand for hydrogen or C¿1?-C8-alkyl, or of a (C1-C8 alkyl) ester of acrylic acid or of methacrylic acid, or mixtures of the styrene compounds and the (C1-C8-alkyl) ester of acrylic acid or methacrylic acid, a2) 0-40 wt.% acrylonitrile or methacrylonitrile or their mixtures, and a3) 0-40 wt.% of one or several other monoethylene unsaturated monomers that are different from a2), B) 1-69 wt.% of a first particle-shaped rubber-elastic polymer B) with a particle diameter d50 of average weight of 300 nm or less, C) 1-69 wt.% of a second particle-shaped rubber-elastic polymer C) with an average-volume particle diameter d50 between 700 nm and 100 νm, whereby the polymer C) is obtainable by the microsuspension polymerization method, by i) dispersion of the monomers corresponding to the polymer C) in water using at least one protective colloid to form a dispersion of droplets with an average-volume particle diameter d50 between 700 nm and 100 νm, and (ii) polymerization of the droplets by means of a radical polymerization initiator, and D) 0-80 wt.% of one or several other polymers. |