Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_715e513cf48b1f74bbc3c816e1c39bbf |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C30B29-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01C7-043 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C30B29-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C30B9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01C7-023 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C30B9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01C7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01C7-02 |
filingDate |
1997-06-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8d9c89531cacb5481ff247e27bde21fd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4e03ca343598781838a393c95935b60c |
publicationDate |
2002-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0906246-A4 |
titleOfInvention |
GROWTH OF NICKEL-COBALT-MANGANESE OXIDE MONOCRYSTALS |
abstract |
The invention relates to the growth of nickel-cobalt-manganese oxide monocrystals having a cubic spinel structure. The relationship between melt composition and crystal composition is shown in the figure for the MO - Mn203 Flux system. MO is equal to the sum of the NiO and CoO components in the system (Average values in mol %). The initial composition of the melt within area ABC is defined by points A, B and C which are given in mol percent. The composition limits of a cubic spinel crystal are defined along the line bounded by points MO and D which are given in mol percent. |