Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dd0864b0569a689eb1fbd8cb67bf405c http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f90c1df3857ee72900e0015c75caecd9 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F1-0573 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C1-0441 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F9-24 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C38-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C38-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F9-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01F1-057 |
filingDate |
1998-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2002-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3ec11199bcc435a7d1b5ed87b13b37ee http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79e569b05586e25ff8e5648e0411475b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_815c058c2646c6af5348f6fb9f0c6d74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_21fb065e4a69585eb0d4832db90897ba |
publicationDate |
2002-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0880148-B1 |
titleOfInvention |
A co-precipitation-reduction-diffusion process for the preparation of neodymium-iron-boron permanent magnetic alloys |
priorityDate |
1997-05-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |