abstract |
The present invention relates to a polymer composition, the 5.0 wt .-%nup to 95.0% by weight of at least one thermotropic liquid-crystalline copolymer, 5.0nWt .-% to 95.0 wt .-% of at least one thermoplastically processablenPolycarbonate and 0.01 wt .-% to 5.0 wt .-% of at least one amplifierncontains. The present invention further relates to a method for producing thenPolymer composition and its use. |