http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0845015-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f76aab74ed312003383a8600e2edbd5b |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2363-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-088 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-02 |
filingDate | 1996-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c7bed7d156bf8b3bf50bf28fd7650271 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac03515a5b69f10ccc5fcb76c2823bcb |
publicationDate | 1998-06-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0845015-A1 |
titleOfInvention | Storage stable autodepositable dispersions of epoxy resins and processes therefor and therewith |
abstract | Epoxy resins, particularly those based on bis-phenol-A, can constitute the principal film forming polymer component of a storage stable autodeposition composition when the particle size distribution of all the film forming polymers in the composition satisfies the following criteria: (1) the mean light scattering particle size is at least about 100 but not more than about 300 nm; (2) no more than about 1.0 % of the light scattering particles volume consists of particles with a diameter larger than about 450 nm; (3) no more than about 25 % of the light scattering particles volume consists of particles with a diameter larger than about 250 nm; (4) no more than about 50 % of the light scattering particles volume consists of particles with a diameter larger than about 200 nm; and (5) no more than about 75 % of the light scattering particles volume consists of particles with a diameter larger than about 175 nm. Such dispersion can conveniently be achieved using a two stage process in which a solution of the film forming polymers is emulsified into water to form a preliminary dispersion and this preliminary dispersion is subjected to at least one particle size refinement stage in which the preliminary dispersion is forced through a narrow aperture. |
priorityDate | 1995-08-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 184.