http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0839616-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a2bcaf91101a370a3d64e3190366357f |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27N3-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27N3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27N3-18 |
filingDate | 1997-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4484fbe9b6a2a3056100433878adae80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb11e8c530860189a896c5e4fe66247c |
publicationDate | 1998-05-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0839616-A2 |
titleOfInvention | Method for preparing wood particle boards with an organic binder |
abstract | A method for the production of wood materials from lignocellulose-containing particles and organic binders is described. The process is characterized in that a fleece remains in the hot press in an overcompressed state corresponding to 0.80 ... 0.98 · d target for the period of 20..90 s. The period of time should, however, be at least until a change in the physical state of the water from the liquid phase to the vapor phase has taken place in the cover layers moistened by spraying on 50-100 g of water per fleece side. The energy content of the steam should be sufficient to initiate a spontaneous temperature increase T of at least 15 ° C in the middle of the fleece when the distance between the press plates is increased to the target thickness of the plate (d target ). |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6533889-B2 |
priorityDate | 1996-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 22.