http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0823398-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7c519c2cc19da16c62613a5c8b6bde0d |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-11 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-23 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-225 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B31-04 |
filingDate | 1996-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_850e5c4e495b7d3fe29641cb025ab5ea http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_be923b3df786853fb0790140558a03e5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_05cfb694a0721132e2e5b1c671afdc03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bcc4e23d484c07499455f99fd1d49c12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6a5e4da9a74618b91168af9d1ab90d53 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2b5eec4ebd86b2b3f927f6ae52c141f1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_88e7310e25fd00b14c6fc00585080fb0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5ea272b8e12bd54f58afb6f7544deef8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7cc801c1538e394d0f27cf6d097e06cf |
publicationDate | 1998-02-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0823398-A1 |
titleOfInvention | Process and device for obtaining oxidised graphite |
abstract | The invention pertains to the technology of carbon-graphite materials, in particular to thenproduction of oxidised graphite used as a component of fireproofing materials, and also to thenproduction of expanded graphite with a high degree of expansion, used in metallurgy, thermalnpower engineering, chemical industry and other industries. n The process of obtaining the oxidised graphite comprises the treatment of powder graphite innan electrolytic solution of strong acids to produce the GIC, hydrolysis, washing and drying thenoxidised graphite. The treatment is conducted in the presence of chemical oxidants at a constantnredox potential 0.55-1.55 V or/and treatment is conducted by anodic oxidation of graphite whilenpassing the electric current through the mixture of graphite and acid placed between anode andncathode at a constant anode potential 1-2 V and in a weight acid-to-graphite ratio of 1-4. As anstrong acid sulphuric or nitric acids are used mainly. n The device for obtaining oxidised graphite comprises reactor with housing having inner cylindricalnsurface. Anode, cathode and the permeable for acid solution diaphragm located betweenncathode and anode are inserted in the housing. Also inserted in the housing are vanes,nwhich are radially fixed on the axial horizontal shaft and have an opportunity of rotation and radialnmoving against the stop to a surface of the anode. Half-ring-shaped situated in the lower partnof the housing between pipes for loading and unloading. The anode is a half-ring whose axis isnshifted against horizontal shaft axis with the gap between anode and diaphragm increasing 1.5-3ntimes from loading to unloading pipe. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1873116-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/GB-2367291-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1873116-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102286753-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1296893-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1296893-A1 |
priorityDate | 1995-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 48.