http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0798796-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_424db9d56b06a23aed410fcf5df652f3 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-32 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B3-0047 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B3-0057 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-383 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C19-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-24 |
filingDate | 1997-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d4cb8457494485741d9a2889d350f159 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a9ddf3d6964cfa6ed9011afab6fb4a05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2e37e8e477fae895ceceb095224adbf2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e1d6ad744fcb6efc625f2ab9d3f82ee3 |
publicationDate | 1997-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0798796-A2 |
titleOfInvention | Rare earth element-containing hydrogen storage alloy, method of producing the same, negative electrode using said alloy, and alkaline rechargeable battery using said electrod |
abstract | Provided is a rare earth element-containing hydrogen storage alloy which fulfills at least one requirement selected from the requirements that (1) the total content of nonmetal elements present as impurities in the alloy matrix is not higher than 1,200 ppm by weight, (2) the total content of alkaline earth metal elements present as impurities in the alloy matrix is not higher than 100 ppm by weight, (3) the content of Mg present as an impurity in the alloy matrix is not higher than 80 ppm by weight, (4) the content of Cl present as an impurity in the alloy matrix is not higher than 10 ppm by weight, (5) the content of Pb present as an impurity in the alloy matrix is not higher than 100 ppm by weight, (6) the alloy has, in a surface layer covering from the alloy surface to a depth of 20 nm, an oxygen concentration that decreases sharply in the depth direction and is not higher than 10 weight % on the average in the surface layer defined above, (7) the alloy comprises Ni as a constituent element and contains, in a surface layer covering from the alloy surface to a depth of 20 nm, oxygen-combined Ni atoms in a proportion sharply decreased in the depth direction the average of which is not higher than 5 weight % to the total Ni atoms in the surface layer defined above, and (8) the surface hardness of the alloy is at least 600 kg/mm 2 in terms of Vickers hardness. n Further, there are described a process of producing the aforesaid hydrogen storage alloy, a negative electrode using the hydrogen storage alloy defined above and an alkaline rechargeable battery using such a negative electrode. |
priorityDate | 1996-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 46.