http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0787231-A4
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_60da379fb33c192ef77f86a60c5ac029 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cea139ad438b9ce7d33159d45b154c6b |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21C9-1063 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21C9-1057 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21C3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08H8-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21C9-147 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21C9-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21C9-153 |
filingDate | 1995-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1997-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0787231-A4 |
abstract | A method for oxidative degradation of lignin and polysaccharide fragments dissolved during polyoxometalate delignification or bleaching of wood pulp, wood fiber or pulp obtained from a non-woody plant. The method comprises the steps of obtaining a spent polyoxometalate bleaching solution containing a polyoxometalate of the formula [VlMomWnNboTap(TM)qXrOs]x- where 1 is 0-18, m is 0-40, n is 0-40, o is 0-10, p is 0-10, q is 0-9, r is 0-6, TM is a d-electron-containing transition metal ion, and X is a heteroatom which is p or d block element, provided that l+m+n+o+p>/=4, l+m+q>0 and s is sufficiently large that x>0, and heating the solution in the presence of an oxidant under conditions wherein the dissolved organic compounds are oxidatively degraded to volatile organic compounds and water. |