Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03627f82d4edc6567f9627df6efdde5d |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-0236 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G8-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G8-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G8-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-004 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G8-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G8-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G8-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G8-00 |
filingDate |
1995-08-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_522dcc9ae8bf04672ff3b0cfc51b3341 |
publicationDate |
1997-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0777694-A1 |
titleOfInvention |
Metal ion reduction in novolak resin solution using an anion exchange resin |
abstract |
The present invention provides methods for producing water insoluble, aqueous alkali soluble novolak resins having a very low level of metals ions, utilizing a specially treated anion exchange resin. A method is also provided for producing photoresist composition having a very low level of metal ions from such novolak resins and for producing semiconductor devices using such photoresist compositions. |
priorityDate |
1994-08-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |