http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0752448-A3

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c7ad58d3c0b071069a8ee0cb8c8ba2e8
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-12
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L69-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-00
classificationIPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-12
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00
filingDate 1996-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3973d4d9a226f06bc02be6eaa70404ee
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fc8a07500c73acb394b54ba632cda86e
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_363851702e599f7141c917832e14148a
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b615b7f21d69a56d8ea6945699ff6125
publicationDate 1998-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber EP-0752448-A3
titleOfInvention Impact modified thermoplastic molding composition containing a silicone rubber powder
abstract The impact strength of a thermoplastic molding composition containing thermoplasticnpolymers selected from the group comprising aromatic polycarbonate, andnthermoplastic (co)polyester, polyamide and copolymer is improved upon thenincorporation therewith of a particular silicone rubber powder. The silicone rubbernpowder, added at a level of about 1 to 25 contains a mixture of (a) a polydiorganosiloxanenand (b) finely divided silica filler.
priorityDate 1995-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5391594-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-8603213-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0505869-A2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0006521-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-2083014-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0260004-A2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0543597-A2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08109262-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0541988-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-T941003-I4
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0596734-A1
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID24261
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457707758

Total number of triples: 41.