Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ba045776bcd32d32e3100da8dfce4e28 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-04 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-914 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D167-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-9155 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D167-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-305 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 |
filingDate |
1994-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_00ddc7cdba5c74d606cfc549e9ac2878 |
publicationDate |
1996-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0746585-A1 |
titleOfInvention |
Process for preparing films and coatings |
abstract |
Extrusion films and coatings are prepared by applying a polyhydroxyalkanoate (PHA) to a surface which is in the range from 20 DEG C above to 20 DEG C below the optimum crystallisation temperature of the PHA. A PHA of high melt flow index is preferred. |