http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0705315-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c721fe8dc4d1b8f924e7e673bd5c2edb |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-16 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J123-34 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-34 |
filingDate | 1993-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d27a1455a607c4796dfe68f9e6add5a8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_260fb2edfec16db2dabdd7c8ac6ee772 |
publicationDate | 1996-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0705315-A1 |
titleOfInvention | Acrylonitrile-butadiene copolymer rubber adhesive |
abstract | An aqueous adhesive composition for bonding nitrile rubber. The adhesive composition contains a chlorosulfonated polyethylene latex, a polyhydroxy phenolic resin copolymer, and a high molecular weight aidehyde polymer. The adhesive composition exhibits an unusual affinity for nitrile rubber and exhibits excellent adhesive performance as a single-coat formulation. The adhesive composition withstands high temperature bonding conditions and minimizes the utilization of volatile organic solvents. |
priorityDate | 1992-05-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |