abstract |
A resin composition comprising polyvinyl alcohol and an inorganic layered compound having an aspect ratio of from 50 to 5,000, wherein the volumetric ratio of the inorganic compound to the polyvinyl alcohol ranges from 5/95 to 30/70; and a laminate and a laminated film each having a layer (1) comprising the above composition or a part of the layer in at least part of the same. The composition, laminate and laminated film exhibit good gas-barrier properties while substantially retaining the good film strength. |