Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0efa077d881a96aeb1e29b21ef1bbb58 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F30-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F30-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-10 |
filingDate |
1994-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bc35db1046db2c22f819f8c84bb00226 |
publicationDate |
1995-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0652238-A2 |
titleOfInvention |
Process for preparing polymers of esters of vinyl phosphonic acid |
abstract |
A monomer mixture consisting mainly of vinylphosphonic acid esters of methanol and / or ethanol is radically polymerized using a salt of peroxodisulfuric acid as a polymerization initiator at a polymerization temperature of 80 to 150 ° C. in aqueous solution. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3901181-A4 |
priorityDate |
1993-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |