Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_aa4fe519fdb71979341cbd808c388542 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-17 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01F7-021 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F7-021 |
filingDate |
1993-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86fc6e352ac02ff0cc6447ebf5d30041 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6e17f70c8d284dac4bbb928fe0447b06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1233f664cd4d2882e42fae45c854a5d |
publicationDate |
1995-06-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0630355-A4 |
titleOfInvention |
PREPARATION OF ALUMINUM OXIDE WITH INCREASED POROSITY. |
abstract |
A process for making high porosity boehmite alumina comprising forming an aqueous dispersion of a boehmite alumina which has been obtained by hydrothermally treating an aqueous mixture of a precursor boehmite alumina at a pH of from about 5 to about 9 for a period of time sufficient to convert the greater portion of the precursor boehmite alumina to a colloidal sol, treating the dispersion of the hydrothermally treated alumina to form a viscous gel and subjecting the gel to sufficient shearing force for a sufficient period of time to increase the pore volume by at least 30 % and the median pore radius by at least 20 %. |