http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0628604-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c478e33e24d9d6818bc28ef57b0bb44d |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-20 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 |
filingDate | 1994-06-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5c12d09a744c2b840d5d3e456702e0e7 |
publicationDate | 1994-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0628604-A2 |
titleOfInvention | Curable compositions |
abstract | A composition comprising an alkenyl polysiloxane having not less than two alkenyl groups per molecule and a polysiloxane having not less than two silicon-bonded hydrogen atoms per molecule. The alkenylpolysiloxane comprises a mixture of polysiloxanes having a viscosity at 25°C of not greater than 10 Pa.s. one having not more than two alkenyl groups per molecule another having not less than three alkenyl groups per molecule. The polysiloxane having not less than two silicon-bonded hydrogen atoms per molecule has a viscosity at 25°C of not greater than 10 Pa.s. and no more than two silicon-bonded hydrogen atoms per molecule. The compositions are of low initial viscosity and yet cure to give elastomers with good strength and elongation to break. The compositions are useful, for example, as mould making materials. |