http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0596438-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_05b4efc837d7b25b7f7c4a7314389f8f |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C1-002 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C1-00 |
filingDate | 1993-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_109c55fa04ad1aaaa8d668cfa98eb4f1 |
publicationDate | 1994-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0596438-A2 |
titleOfInvention | Method of solidifying filter residues containing heavy metals |
abstract | For solidifying waste or residues containing heavy metals by means of glazing or sintering for subsequent disposal or reuse, the waste or residues are mixed with at least one glass-forming and / or glass-converting substance and / or with a melt accelerator so that the The melting point of the waste or residues is reduced. The method according to the invention is particularly suitable for solidifying filter dust or flue gas cleaning residues from combustion plants, the melting point being lowered below 1000 ° C. by the addition of the substances and / or the accelerator, and the vitrification or sintering in a temperature range, preferably from 700 to 900 ° C, is done. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008539053-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7645095-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021012043-A1 |
priorityDate | 1992-11-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 46.