abstract |
A process for preparing polymers having molecular weights below 5,000 and polydispersity below 2.5 is provided. The polymerization is conducted in supercritical carbon dioxide at temperatures of at least 200 DEG C and pressures above 3,500 psi. The process can be continuous, semi-continuous, or batch. The polymers are useful as detergent additives, scale inhibitors, dispersants and crystal growth modifiers. |