http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0590210-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_050503c7182014159e0d0511e3cb88e2 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B20-008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B14-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B20-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-08 |
filingDate | 1992-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f17c5f111160c2ce51df445644259be3 |
publicationDate | 1994-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0590210-A1 |
titleOfInvention | High performance mortar or concrete |
abstract | The subject of the invention is the production of a high performance mortar or concrete, and in particular the crushing strength of which can exceed 40 MPa, such a mortar or concrete comprising, in desired proportions, a cement, solid aggregates and any additives, the whole being mixed and then adding water.n n n According to the invention, the siliceous product consists of a fine powder obtained by simple disintegration of a natural Diatomite taken in quarry to a degree of fineness between 0.1 and 100 μm, and capable of replacing part of the cement of equal strength, said powder being present in a proportion of at least 7% of the weight amount of cement. |