Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ccfba36bede615686c297ad796fcc3ab |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C16-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C16-0281 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C16-27 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B41-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C16-27 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C16-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C16-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C30B29-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C16-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C30B25-02 |
filingDate |
1993-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7107af718c2e519a1dfd14ff75aaaac7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a6b2e9c78e37ed121a346861284667b6 |
publicationDate |
1993-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0556615-A2 |
titleOfInvention |
Method of making synthetic diamond |
abstract |
Deposition of synthetic diamond on a graphite substrate can be substantially improved by providing a thin interlayer of a metal, particularly molybdenum or tungsten. The preferred thickness of the metal layer is about one to two times the maximum pore size. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/GB-2304982-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016128883-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0693573-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0622473-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5821544-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5527559-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/GB-2304982-B |
priorityDate |
1992-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |