Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a2973a1bdaf87d5184fb1e81ebe5d061 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L59-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-02 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L59-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L59-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L57-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 |
filingDate |
1992-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f569d2aa829eb814d4636d534bb6737d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a18dfaa7c28a4c8dc59bf1c6b24595a3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dddee56fff734206bfdde89c14d3f894 |
publicationDate |
1993-01-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0522180-A1 |
titleOfInvention |
Structure of polyacetal-base resin composiiton and production thereof |
abstract |
A structure of a polyacetal-base resin composition comprising a polyacetal resin and a polyolefin resin added thereto to form a network structure wherein both resins are dispersed in each other and which has good acid resistance and fusibility with a polyolefin resin and excellent mechanical properties. In the step of melt mixing the polyacetal resin (A) as a matrix with the polyolefin resin (B), a filler (C) having a surface tension at least greater than that of the component (B) at the melt mixing temperature and a mean particle diameter of 0.05 to 50 µm is added in such an amount as to satisfy the relation represented by equations (1): B/(A+B)=0.05-0.5 (by weight) and (2): C/(B+C)=0.1-0.7 (by weight) . |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6936651-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6977117-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2004058886-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6391956-B1 |
priorityDate |
1991-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |