Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f6e960aa6ad2ba6401030159343ebe68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dca153f19868f747eeea612b047a9e7c |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-263 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-0001 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-00 |
filingDate |
1992-06-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5ea1c1077cec9960ced51930ab614db9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_40ebd59fe78c75cee03c244c780ccc7d |
publicationDate |
1992-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0518231-A2 |
titleOfInvention |
Process for the preparation of substrates for optical disk |
abstract |
A process for the preparation of substrate for optical disk characterized in that pellets of n 4-methyl-1-pentene polymer or copolymer having a melt flow rate (MFR), as measured according to ASTM D1238 under a load of 5 kg and at a temperature of 260°C, of 240-1200 g/10 min, and a melting point as measured by means of DSC of 234-240°C, nare injection molded into the substrate under the conditions where a temperature of at least part of a cylinder is 320-370°C and a mold temperature is not more than 55°C. |