Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_af7c9c966acd2ef7eca105d82d8d0991 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L81-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-09 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L87-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L81-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 |
filingDate |
1991-07-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a1ff4c2069040375be484e855962d5a8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2ab5a5ede3b5fe7a64805a77c7b613b1 |
publicationDate |
1992-01-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0466099-A1 |
titleOfInvention |
Use of polyethylene in poly(arylene sulfide) composition for reducing shrinkage |
abstract |
There are provided compositions comprising poly(arylene sulfide), polymeric rubber, polyethylene, and carboxylic anhydride; and methods for making these compositions. Articles produced from the compositions have reduced shrinkage and improved impact strength. |