http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0450977-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C2001-7451 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-015 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-95 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-95 |
filingDate | 1991-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6e763ec783e17da765aef081cc76c776 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82586d7c0fc1751e5c74831bddcc693b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eef9165d91558bb3e082a8773aac867b |
publicationDate | 1991-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0450977-A2 |
titleOfInvention | Process for producing silver halide photographic materials |
abstract | A process for producing a silver halide photographic material containing a support which has a first side and a second side, a light-sensitive silver halide emulsion layer on said first side, a first hydrophilic colloidal layer on said emulsion layer and a second hydrophilic colloidal layer on said second side, comprising: n providing said first hydrophilic colloidal layer on said emulsion layer, n providing said second hydrophilic colloidal layer on said second side, nand n drying said first hydrophilic colloidal layer and said second hydrophilic colloidal layer simultaneously, n wherein said first hydrophilic colloidal layer and said second hydrophilic colloidal layer have a matting agent with a particle size of not less than 4 µm in an amount of not less than 4mg/m², n wherein said first hydrophilic colloidal layer and said second hydrophilic colloidal layer have a smooster value of not less than 25 mmHg. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0679938-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0679938-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0773472-A1 |
priorityDate | 1990-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 194.