http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0439079-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c6430c90005b67a61bc434a2115964d2 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S525-904 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F255-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-00 |
filingDate | 1991-01-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1996-04-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_56754eb69a9d0b62230f7d962b7f7615 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2b7744b427d5473bd00146a5b6708a04 |
publicationDate | 1996-04-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0439079-B1 |
titleOfInvention | Method of producing olefin polymer graft copolymers |
abstract | Disclosed is a method of making graft copolymers of olefin polymers by contacting a particulate olefin polymer with a free radical polymerization initiator, e.g., a peroxide, and a vinyl monomer at about from 60 DEG to 125 DEG C, while controlling the monomer addition rate so that it does not exceed about 4.5 pph/min, and most preferably does not exceed about 3.0 pph/min, at any monomer feed level. To prevent polymer degradation, a non-oxidizing environment is maintained throughout the process, and residual free radicals are deactivated, and unreacted initiator is decomposed, before the graft copolymer is exposed to air. |
priorityDate | 1990-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 159.