Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1e70c0aeade92d7571d955d3b90ea06e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2071-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2365-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D7-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-022 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K71-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29D7-01 |
filingDate |
1990-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1995-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ea19da3d5aa6518745ff75c7d2e813a1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7f8c4247cb6b27e62422a5cc30dba261 |
publicationDate |
1995-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0434323-B1 |
titleOfInvention |
Process for making continuous films of ordered poly(aryl-ether-ketone-ketones) |
abstract |
A process for extruding a smooth and uniform film or sheet of an ordered poly(ether ketone ketone) having a thickness of about 2.5 to 250 micrometers, wherein the molten extrudate is quenched on a drum maintained at a temperature of about 100-170 DEG C. <IMAGE> |