Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4eefac142a032449aa6a1a51fadaf766 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2962 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-2008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2938 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-2992 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K1-0366 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C25-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-08 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K1-03 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C25-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C25-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-08 |
filingDate |
1990-11-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b2c3080272fcbcbe8f7394bea5f76c1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4312ff1add251a1c0785a26a29f74db0 |
publicationDate |
1991-06-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0431333-A1 |
titleOfInvention |
Method for producing glass cloth |
abstract |
The present invention provides a method for producing a glass cloth which is suitable as reinforcing material for making resin laminates and which comprises subjecting filaments of glass fibers to sizing treatment with a sizing agent containing at least one water-soluble film forming agent selected from the group consisting of an amine-modified epoxy resin, an ethylene oxide-added epoxy resin and ethylene oxide-added bisphenol A as film forming component, forming glass yarns from the thus treated filaments, weaving the glass yarns to make a glass cloth, washing the glass cloth with water until LOI of the sizing agent to the glass cloth reaches 0.25% by weight or less, and then treating this glass cloth with a solution of a surface treating agent. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2006043019-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0578974-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107532348-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0578974-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8501309-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112760782-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109721752-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109721752-A |
priorityDate |
1989-11-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |