Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ea48a63bf803801352b775dd71e13b72 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2096-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2029-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C33-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C37-0071 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B26D7-088 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D5-08 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C37-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B26D7-08 |
filingDate |
1990-07-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6651cb60f78b78121cc02e8f7762eb86 |
publicationDate |
1991-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0412867-A1 |
titleOfInvention |
Process for the continuous antiadhesive treatment of an adhesive band, especially of a thermoplastic, extruded adhesive, and also the device for its processing and the corresponding product |
abstract |
The invention relates to a method of continuous non-stick treatment of a bead of permanent adhesive material, more particularly of a hot-melt adhesive exiting from an extruder mixer or from a die at a temperature above its softening temperature, process characterized in that a coating of an anti-adhesive agent compatible with the constituent material thereof and not causing any physico-chemical modification of this material is applied to at least part of the surface of the bead the bead thus coated is cooled, then it is cut to the desired length and the fragments thus obtained are directly conditioned, without additional precautions.n n n The invention also relates to an installation for implementing this method. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5443903-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6230890-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6044625-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9600747-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6006497-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-2704162-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0603456-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1878551-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9423921-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5865927-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5401455-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5373682-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0749820-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/AU-686828-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5819505-A |
priorityDate |
1989-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |