Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c7ad58d3c0b071069a8ee0cb8c8ba2e8 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D9-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D9-0013 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D9-00 |
filingDate |
1989-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c400ad8145aa25b11e0e7b82a1ea9d0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_46631305c14be78fa17dfba109dfbde6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d8c041a5186d31eafc87190c04506faa |
publicationDate |
1990-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0354433-A2 |
titleOfInvention |
Process for separating substances by cool chrystallization |
abstract |
In the process for material separation based on the principle of cooling crystallization, after the crystal layer has been deposited in the crystallizer, the remaining mixture is removed and the crystal layer is melted off. The process is characterized in that the mixture which completely fills the crystallizer is set in vibration during the solidification by forced oscillatory movements and is left in the crystallizer until a degree of solidification of 50% to 90% is reached. |
priorityDate |
1988-08-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |