Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_28a869d6fc950d50f6df03f549ca3afa |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-384 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B32-384 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B32-336 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10C3-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B31-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F27B15-00 |
filingDate |
1988-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_69cfd9cfd77990b668301ca4d54d95c7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cb8ab72688977d737d4205ccd003b49d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f89ec702d1a555ab2c8955d0fa0abec1 |
publicationDate |
1989-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-0317217-A2 |
titleOfInvention |
Method and apparatus for activating infusibilized pitch beads |
abstract |
A method of and an apparatus for calcining and activating infusibilized spherical pitch beads wherein the beads (6), which have been prepared by infusibilizing spherical beads of a petroleum pitch or a coal pitch, are calcined and activated in a furnace comprising a first fluidized bed (2) in which the beads are calcined at a temperature of from 600 to 800°C and a second fluidized bed (3) in which the thus calcined beads are activated at a temperature of from 800 to 1,200°C. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0458548-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1897852-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1897852-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5370794-A |
priorityDate |
1987-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |