http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0261175-A4
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_699439deb18b3a48be0346ef00d950f1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7808f1bf4788004c5916b3dc70ec2c46 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H1-60 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-58 |
filingDate | 1987-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_582f3c4c9c6b941fb427d918f48065a1 |
publicationDate | 1988-07-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-0261175-A4 |
titleOfInvention | FIBER PULP AND MANUFACTURING. |
abstract | A process for bonding fibers comprising the steps of contacting the fibers with a particulate plastic alloy. The plastic alloy comprises a compound and a thermoplastic resin. The compound must be a crystalline organic compound, must have a melting point of 20 to 200 DEG C, must have a boiling point of 100 to 450 DEG C and must be a solvent for the resin. The mixture of the plastic alloy and the fibers are heated to melt the alloy and bind the fibers. |