abstract |
The rubber flooring according to the present invention is used for vehicles and floors of buildings. It is compounded with at least 40 weight parts of aluminium hydroxide, at least 10 weight parts (as metal quantity) of at least one selected from among calcium carbonate, magnesium carbonate, magnesium oxide, calcium hydroxide and magnesium hydroxide and at least 3 weight parts of at least one selected from among zinc borate, antimony trioxide and antimony pentoxide, to 100 weight parts of rubber. It has both flame-resistance and low fuming property. |